Nimonic 75
Nimonic 75
Common Trade Names:UNS N06075,W.Nr2.4951/2.4630
Nimonic 75Chemical Composition:
Alloy |
% |
C |
Cr |
Ni |
Ti |
Fe |
Cu |
Mn |
Si |
75 |
Min. |
0.08 |
18 |
Bal. |
0.2 |
|
|
|
|
Max |
0.15 |
21 |
0.6 |
0.5 |
0.5 |
1 |
1 |
Nimonic 75Physical properties:
Density |
8.37g/cm3 |
Melting point |
2450-2520°C |
Nimonic 75minimum mechanical properties in the room temperature:
Alloy |
Tensile strength |
Thermal conductivity |
Coefficient of thermal expansion |
Hardness HB |
|
Rm N/mm2 |
W/m• °C |
μm/m/°C |
|||
Nimonic 75(solution) |
1400-2210 |
11.7 |
11 |
241 |
Availability
Alloy 75 is available in Bar, Plate, Strip, Sheet, Wire,TubeRod, Forging Stock and Extruded Section. For all stock availability contactsales.
Specifications
Rod, Bar, Wire and Forging Stock |
BSHR 5, BS HR 504, DIN 17752, AECMA PrEN2306, AECMA PrEN2307, AECMA PrEN2306, AECMA Pr EN2307, AECMA PrEN2402, ISO 9723, ISO 9724, ISO 9725 |
Plate, Sheet, Strip |
BS HR 203, DIN 17750, AECMA PrEN2293, AECMA PrEN2302, AECMA PrEN2411, ISO 6208 |
Pipe and Tube |
BS HR 403, DIN 17751, AECMA PrEN2294, ISO 6207 |
Other |
DIN 17742, AECMA PrEN2308, Werkstoff Nr 2.4630, W. Nr 2.4951, UNS N06075, Nimonic 75 (tradename), MSRR 7104 and MSRR 7004, AFNOR NC 20T |
Typical Mechanical Properties Alloy 75
Rupture Strength (1000 h) |
||
Temperature |
psi |
MPa |
760°C/ 1400° F |
6000 |
40 |
815°C/1500 °F |
3500 |
24 |
870°C/1600 °F |
2200 |
15 |
925°C/1700 °F |
1500 |
10 |
980°C/1800 °F |
1200 |
8 |
(This material was Annealed)